Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 120 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 100 - 120 MPa

@Temperature 1300 °C
14500 - 17400 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 130 Dense Vibrating Refractory Castable
Description: Vibron 130 is a vibrating castable with a low cement content, based on abrasion resistant spinel grains.Remarks: Indicated values apply to vibrated products.Information provided by Goud..
Compressive Strength 100 - 120 MPa

@Temperature 1300 °C
14500 - 17400 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 140 Dense Vibrating Refractory Castable
Description: Vibron 140 is a low cement castable, based on high quality chamotte.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast.
Compressive Strength 100 - 120 MPa

@Temperature 1400 °C
14500 - 17400 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 160 Dense Vibrating Refractory Castable
Description: Vibron 160 is a low cement vibrating castable on andalusite base, characterized by a high strength and excellent thermal shock resistance.Remarks: Indicated values apply to vibrated pro..
Compressive Strength 100 - 120 MPa

@Temperature 1400 °C
14500 - 17400 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 160 H Dense Vibrating Refractory Castable
Description: Vibron 160 H is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance.Remarks: Indicated values apply to vib..
Compressive Strength 100 - 120 MPa

@Temperature 1400 °C
14500 - 17400 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable
Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide..
Compressive Strength 100 - 120 MPa

@Temperature 1400 °C
14500 - 17400 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 170 M Dense Vibrating Refractory Castable
Description: Vibron 170 is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags.Remar..
Compressive Strength 100 - 120 MPa

@Temperature 1400 °C
14500 - 17400 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 160 H RAPID Dense Vibrating Refractory Castable
Description: Vibron 160 H Rap is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance. Because of special additives, thi..
Compressive Strength 100 - 120 MPa

@Temperature 1400 °C
14500 - 17400 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable
Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1..
Compressive Strength 100 - 120 MPa

@Temperature 1400 °C
14500 - 17400 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 160 K Dense Vibrating Refractory Castable
Description: Vibron 160 K is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity and high abrasion resistance. The thermal shock resistance is excell..
Compressive Strength 100 - 120 MPa

@Temperature 1400 °C
14500 - 17400 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable
Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidatio..
Compressive Strength 100 - 120 MPa

@Temperature 1400 °C
14500 - 17400 psi

@Temperature 2550 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 170 M RAPID Dense Vibrating Refractory Castable
Description: Vibron 170 M Rapid is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sla..
Copyright © lookpolymers.com All Rights Reserved