Material Notes:
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminated with plastics, metals, adhesives, and other materials. Every SPREADERSHIELD™ part is customized to meet specific application needs and improve thermal performance within a limited space and weight. SPREADERSHIELD™ products have provided thermal solutions in a variety of industries and applications, including displays (PDP, LCD CCFL, LED BLU, OLED), cell phones, laptop and ruggedized computers, handheld gaming devices, batteries, projectors, set-top boxes, and automotive electronics. Each application is specialized to require different characteristics of SPREADERSHIELD™ products. Grade SS600 is designed specifically for handsets, Pico-projectors, and cameras.
Physical Properties Metric English Comments
Thickness 100 microns
3.94 mil
Standard
100 - 127 microns
3.94 - 5.00 mil
Available Range
127 microns
5.00 mil
Standard
Mechanical Properties Metric English Comments
Tensile Strength at Break 9.70 MPa
1410 psi
Thermal Properties Metric English Comments
CTE, linear -0.400 µm/m-°C
-0.222 µin/in-°F
In-Plane
27.0 µm/m-°C
15.0 µin/in-°F
Through-Plane
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
Thermal Conductivity 3.50 W/m-K
24.3 BTU-in/hr-ft²-°F
Nominal, Through-Plane; ASTM-D5470 Modified Method
600 W/m-K
4160 BTU-in/hr-ft²-°F
Nominal, In-Plane; Angstrom's Method
Maximum Service Temperature, Air 400 °C
752 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Electrical Resistivity 0.000340 ohm-cm
0.000340 ohm-cm
In-Plane
0.100 ohm-cm
0.100 ohm-cm
Through-Plane
Descriptive Properties Value Comments
Thermal Contact Impedance - Per Side (°C·cm²/W) 0.44
at 0.10 mm spreader thickness