Material Notes:
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183/A
Moisture Absorption at Equilibrium <= 0.25 %
<= 0.25 %
Karl-Fischer; ISO 15512/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527
Elongation at Break 130 %
130 %
ISO 527
Elongation at Yield 4.0 %
4.0 %
ISO 527
Tensile Modulus 1.90 GPa
276 ksi
ISO 527
Flexural Strength 55.0 MPa
7980 psi
ISO 178
Flexural Modulus 1.30 GPa
189 ksi
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 7.50 J/cm²

@Temperature 23.0 °C
35.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75/A
Vicat Softening Point >= 200 °C
>= 392 °F
50N; ISO 306