Material Notes:
Silver Ink C2000107P3 is designed as a termination for single layer PZT ceramics. After firing the film has good adhesion and solderability.The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 71 %
71 %
Particle Size 4.0 µm
4.0 µm
Main Break; Fineness of Grind
6.0 µm
6.0 µm
3rd Streak; Fineness of Grind
Viscosity 11000 - 19000 cP

@Shear Rate 100 1/s,
Temperature 25.0 °C
11000 - 19000 cP

@Shear Rate 100 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer (PK1.1°)
Storage Temperature 20.0 °C
68.0 °F
Processing Properties Metric English Comments
Processing Temperature 150 °C
302 °F
Cure Time 10.0 - 15 min
0.167 - 0.25 hour
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 150
230 mesh stainless steel screen
Printing Mesh counts/inch 180 to 340
stainless steel or polyester screens