Gwent Electronic Materials C2031105D2 Palladium Ink

Category Fluid , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2031105D2 Palladium Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Palladium Ink C2031105D2 is an ink formulated for screen printing for use on Fuel Cells. It is suitable for application onto Solid Oxide Fuel Cells.The ink has been made at a ready to use viscosity and should be thoroughly stirred before use avoiding introduction of air bubbles. It can be printed on automatic and semi automatic screen printers.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 70 %
70 %
Particle Size <= 5.0 µm
<= 5.0 µm
Main Break; Fineness of Grind
<= 8.0 µm
<= 8.0 µm
3rd Streak; Fineness of Grind
Viscosity 10000 cP

@Shear Rate 100 1/s,
Temperature 25.0 °C
10000 cP

@Shear Rate 100 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer (PK1.1°)
Storage Temperature 20.0 °C
68.0 °F
Processing Properties Metric English Comments
Processing Temperature 120 - 150 °C
248 - 302 °F
Cure Time 10.0 - 15 min
0.167 - 0.25 hour
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Printing Mesh counts/inch 180 to 340
stainless steel or polyester screens