Gwent Electronic Materials C2100217D1 Aluminium for PTC paste

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2100217D1 Aluminium for PTC paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aluminium Ink designed to give good ohmic contact on to barium titanate PTC components. This product is particularly good where large volumes of PTC components are being processed in belt furnaces conditions, where improved stain resistance and good visual appearance are required. Screen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyesterSubstrate: PTC ceramic partsInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 68 - 72 %

@Temperature 150 °C
68 - 72 %

@Temperature 302 °F
Viscosity 11000 - 18000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
11000 - 18000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C
68.0 °F
sealed container
Processing Properties Metric English Comments
Sintering Temperature 780 - 910 °C
1440 - 1670 °F
Cure Time 15.0 min

@Temperature 150 °C
0.250 hour

@Temperature 302 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 227
Using a 230 mesh stainless steel screen