H.C. Starck HPM 1701 Tungsten High Density Composite

Category Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer H.C. Starck
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck HPM 1701 Tungsten High Density Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for further processing by the customer or in accordance with the drawing as finished machined component.Our HPM 1700 to HPM 1850 materials provide a solution in a wide range of applications requiring concentrated weight or density in a limited space. These lead-free parts meet legal requirements and recommendations to protect the environment.Range of Application: Balance weights, radiation protection, vibration absorbers, heat transfer, drilling bars. The mechanical characteristics have to guarantee the stability and strength in any application case.The absorption of x-ray and gamma radiation is in direct proportion to the density of the shielding material. Tungsten high density composites are more than 1.5 times as effective as lead and provide extremely efficient protection, particularly where space is limited.Information provided by H.C. Starck.
Physical Properties Metric English Comments
Density 16.8 - 17.2 g/cc
0.607 - 0.621 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers <= 320
<= 320
HV 30
Tensile Strength 670 MPa
97200 psi
Tensile Strength, Yield >= 520 MPa
>= 75400 psi
Elongation at Break 3.0 %
3.0 %
Modulus of Elasticity 300 GPa
43500 ksi
Thermal Properties Metric English Comments
CTE, linear 6.00 µm/m-°C

@Temperature 20.0 - 100 °C
3.33 µin/in-°F

@Temperature 68.0 - 212 °F
6.20 µm/m-°C

@Temperature 20.0 - 300 °C
3.44 µin/in-°F

@Temperature 68.0 - 572 °F
6.40 µm/m-°C

@Temperature 20.0 - 450 °C
3.56 µin/in-°F

@Temperature 68.0 - 842 °F
Thermal Conductivity >= 90.0 W/m-K
>= 625 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Tungsten, W 90 %
90 %
Balance - Ni, Cu
Electrical Properties Metric English Comments
Volume Resistivity 0.000012 ohm-cm
0.000012 ohm-cm
Magnetic Permeability <= 1.05
<= 1.05