Material Notes:
Good surface appearance, high temperature resistanceInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183/A
Melt Flow 20 g/10 min
20 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
ISO 868
Tensile Strength at Break 22.0 MPa
3190 psi
ISO R 527
Tensile Strength, Yield 28.0 MPa
4060 psi
ISO R 527
Elongation at Yield >= 100 %
>= 100 %
ISO R 527
Modulus of Elasticity 2.10 GPa
305 ksi
ISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²
2.62 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched NB
NB
ISO 179/IeU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 165 - 168 °C
329 - 334 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75-2/AF
Vicat Softening Point 153 °C
307 °F
ISO 306/A50
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
CEI 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
CEI 60093
Comparative Tracking Index >= 600 V
>= 600 V
CEI 60112/Solution A