Haysite H330 Polyester Composite

Category Polymer , Thermoset , Polyester, TS
Manufacturer Haysite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Haysite H330 Polyester Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A thermoset polyester composite that offers superior energy efficiency, temperature control, and durability for high temperature mold and platen thermal applications. A proven, cost effective product for the plastic and rubber molder. Available in thicknesses from 1/8" - 2.00". Color - Orange.Information provided by Haysite
Physical Properties Metric English Comments
Water Absorption 0.25 %
0.25 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength 82.7 MPa
12000 psi
ASTM D638
Tensile Modulus 11.0 GPa
1600 ksi
ASTM D638
Flexural Strength 157 MPa
22800 psi
ASTM D790
Compressive Strength 303 MPa
44000 psi
ASTM D695
181 MPa

@Temperature 260 °C
26200 psi

@Temperature 500 °F
ASTM D695
211 MPa

@Temperature 204 °C
30600 psi

@Temperature 400 °F
ASTM D695
219 MPa

@Temperature 149 °C
31700 psi

@Temperature 300 °F
ASTM D695
Poissons Ratio 0.332
0.332
ASTM E132
Shear Modulus 4.13 GPa
599 ksi
Calculated
Izod Impact, Notched 6.94 J/cm
13.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 43.0 µm/m-°C
23.9 µin/in-°F
ASTM D696
Thermal Conductivity 1.85 W/m-K
12.8 BTU-in/hr-ft²-°F
ASTM D177
Maximum Service Temperature, Inert 288 °C
550 °F
Users viewing this material also viewed the following: