Material Notes:
Homopolymer and FDA compliant.Features: Very high flow rapid set-up characteristics, excellent clarity, gloss, and stiffness.Applications: Injection molding: lids and difficult to fill applications.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170Information provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Melt Flow 60 g/10 min
60 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Ultimate 9.00 MPa
1310 psi
ASTM D638
Tensile Strength, Yield 12.0 MPa
1740 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Modulus of Elasticity 0.345 GPa
50.0 ksi
Secant; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 98.0 °C
208 °F
ASTM D1525