Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IDI Composites E-203 Thermoset Polyester, Sheet

Category Polymer , Thermoset , Composite SMC , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer IDI Composites
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IDI Composites E-203 Thermoset Polyester, Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resistance. Designed to meet critical impulse and corona specifications.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
Water Absorption 0.10 %
0.10 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 29 - 35
29 - 35
ASTM D2583
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 10.0 GPa
1450 ksi
ASTM D790
Compressive Strength 165 MPa
23900 psi
ASTM D695
Izod Impact, Notched 5.10 J/cm
9.55 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Strength 15.8 kV/mm
401 kV/in
ASTM D149
Arc Resistance 185 sec
185 sec
ASTM D495