Material Notes:
CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD ADHESIVE, HIGH SPEED APPLICATIONS: EXTRUSION COATING FOR COATED WOVEN BAGS AND TARPAULINS
Physical Properties Metric English Comments
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 86
86
ASTM D785
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Yield 35.5 %
35.5 %
ASTM D638
Flexural Modulus 0.750 GPa
109 ksi
1% Secant; ASTM D790
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Heat Distortion Temperature 76.0 °C
169 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 200 - 280 °C
392 - 536 °F