IRPC Polimaxx Polene GA3750 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene GA3750 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHARACTERISTICS: GOOD EXTRUDABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR SHOPPING BAGS, GROCERY BAGS
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
Condition B, F50; ASTM D1693
Melt Flow 0.050 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.050 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
0.25 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
DIN 53505
Tensile Strength at Break 40.5 MPa
5870 psi
ASTM D638
Tensile Strength, Yield 27.5 MPa
3990 psi
ASTM D638
Elongation at Break 1700 %
1700 %
ASTM D638
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 180 - 210 °C
356 - 410 °F