Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer ITW Plexus
Trade Name Plexus™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Density 0.986 g/cc
0.0356 lb/in³
Mixed
Viscosity 50000 - 70000 cP
50000 - 70000 cP
B
100000 - 125000 cP
100000 - 125000 cP
A
Mechanical Properties Metric English Comments
Tensile Strength at Break 12.1 - 13.8 MPa
1750 - 2000 psi
Elongation at Break 90 - 110 %
90 - 110 %
Tensile Modulus 0.414 - 0.552 GPa
60.0 - 80.0 ksi
Shear Strength 8.62 - 11.0 MPa
1250 - 1600 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point 10.6 °C
51.0 °F
TCC
Processing Properties Metric English Comments
Pot Life 4.0 - 6.0 min
4.0 - 6.0 min
Descriptive Properties Value Comments
Color Blue
Fixture Time 15-20 minutes
Gap Filling Max 0.375 in
Mix Ratio 10:1
By volume
Users viewing this material also viewed the following: