Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent low temperature and toughness properties.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
Mixed
Viscosity 40000 - 60000 cP
40000 - 60000 cP
B
135000 - 175000 cP
135000 - 175000 cP
A
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.8 - 17.2 MPa
2000 - 2500 psi
Elongation at Break 100 - 140 %
100 - 140 %
Tensile Modulus 0.207 - 0.276 GPa
30.0 - 40.0 ksi
Shear Strength 10.3 - 13.8 MPa
1500 - 2000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point 10.6 °C
51.0 °F
TCC
Processing Properties Metric English Comments
Pot Life 8.0 - 12 min
8.0 - 12 min
Descriptive Properties Value Comments
Color Off-white, white, or black
Fixture Time 25-30 minutes
Gap Filling Max 0.375 in
Mix Ratio 10:1
By volume