Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ITW Plexus Plexus™ MA922 Methacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer ITW Plexus
Trade Name Plexus™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Plexus Plexus™ MA922 Methacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, medium open time.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Density 0.971 g/cc
0.0351 lb/in³
Mixed
Viscosity 10000 - 20000 cP
10000 - 20000 cP
B
100000 - 125000 cP
100000 - 125000 cP
A
Mechanical Properties Metric English Comments
Tensile Strength at Break 12.4 - 15.2 MPa
1800 - 2200 psi
Elongation at Break 75 - 100 %
75 - 100 %
Tensile Modulus 0.483 - 0.621 GPa
70.0 - 90.0 ksi
Shear Strength 9.65 - 11.7 MPa
1400 - 1700 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point 10.6 °C
51.0 °F
TCC
Processing Properties Metric English Comments
Pot Life 17 - 24 min
17 - 24 min
Descriptive Properties Value Comments
Color Blue
Fixture Time 35-40 minutes
Gap Filling Max 0.375 in
Mix Ratio 10:1
By volume
Users viewing this material also viewed the following: