Imerys Minsparâ„¢ 10 Ground Feldspar

Category Ceramic , Clay , Feldspar Clay
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name Minspar™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys Minsparâ„¢ 10 Ground Feldspar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Minsparâ„¢ 10 is a fine particle size, ground Feldspar with a tightly controlled particle size distribution. Minsparâ„¢ 10 is easily dispersed to a high Hegman grind to produce coatings finishes with high gloss and sheen. The combination of low 325 mesh residue, mean particle size, and exterior durability make Minsparâ„¢ 10 an excellent mineral additive for thin film coating and adhesive applications, interior and exterior paints and coatings and powder coatings systems.Information provided by Imerys
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.561 g/cc
0.0203 lb/in³
loose
0.641 g/cc
0.0231 lb/in³
packed
Density 2.59 g/cc
0.0935 lb/in³
solid
Brightness 93.5 %
93.5 %
G.E. Brightness
Particle Size 3.0 µm
3.0 µm
mean
Particle Mesh Size 325 Mesh
325 Mesh
less than 0.01 retained
pH 9.3
9.3
10% solids
Mechanical Properties Metric English Comments
Hardness, Mohs 6.0
6.0
Optical Properties Metric English Comments
Refractive Index 1.53
1.53
Processing Properties Metric English Comments
Moisture Content 0.10 %
0.10 %
Descriptive Properties Value Comments
Hegman Grind 6.5