Imerys Minsparâ„¢ 7 Ground Feldspar

Category Ceramic , Clay , Feldspar Clay
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name Minspar™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys Minsparâ„¢ 7 Ground Feldspar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Minsparâ„¢ 7 is a fine particle size, ground Feldspar with a tightly controlled particle size distribution. Minsparâ„¢ 7 is easily dispersed to a high Hegman grind to produce coatings with high gloss and sheen. The combination of low 325 mesh residue, particle size, and exterior durability make Minsparâ„¢ 7 an excellent mineral additive for interior and exterior non-flat coatings, adhesives, sealants and caulk compounds.Information provided by Imerys
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.641 g/cc
0.0231 lb/in³
loose
0.881 g/cc
0.0318 lb/in³
packed
Density 2.59 g/cc
0.0935 lb/in³
solid
Brightness 92 %
92 %
G.E. Brightness
Particle Size 5.0 µm
5.0 µm
mean
Particle Mesh Size 325 Mesh
325 Mesh
less than 0.01% retained
pH 9.3
9.3
10% solids
Mechanical Properties Metric English Comments
Hardness, Mohs 6.0
6.0
Optical Properties Metric English Comments
Refractive Index 1.53
1.53
Processing Properties Metric English Comments
Moisture Content 0.10 %
0.10 %
Descriptive Properties Value Comments
Hegman Grind 6