Indium Corp. Indalloy 144 Tin-Lead Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 144 Tin-Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.88 g/cc
0.357 lb/in³
Thermal Properties Metric English Comments
Melting Point 184 - 263 °C
363 - 505 °F
Solidus 184 °C
363 °F
Liquidus 263 °C
505 °F
Component Elements Properties Metric English Comments
Antimony, Sb 1.3 %
1.3 %
Lead, Pb 73.7 %
73.7 %
Tin, Sn 25 %
25 %