Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 235 - 263 °C
455 - 505 °F
Average value: 254 °C Grade Count:9
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
Melting Point 255 - 263 °C
491 - 505 °F
Average value: 259 °C Grade Count:65
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Melting Point 221 - 263 °C
430 - 505 °F
Average value: 256 °C Grade Count:11
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Melting Point 184 - 263 °C
363 - 505 °F
Indium Corp. Indalloy 144 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Melting Point 255 - 263 °C
491 - 505 °F
Average value: 259 °C Grade Count:11
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..