Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos J50-1000-178 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos J50-1000-178 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A high density polyethylene copolymer intended for the injection molding of closures for beverages. Because of its high purity and excellent organoleptic properties, this grade is certified as low taste and is intended for packaging in direct contact with beverages. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ASTM D4883
Environmental Stress Crack Resistance 4.0 hour
4.0 hour
ASTM D 1693A
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 190 °C
11 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 25.5 MPa
3700 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break >= 500 %
>= 500 %
2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 1.207 GPa
175.1 ksi
Tangent; ASTM D 790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
ASTM D648
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Injection Molding
Region US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: