Ineos N05G-00 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos N05G-00 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade N05G-00 is a general purpose high impact copolymer polypropylene for injection molding applications. It offers a superior balance of stiffness and impact strength as compared to competitive impact copolymers of similar melt flow rate. This material meets the requirements of the U. S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsAppliances Automotive Consumer products Rigid packaging HousewaresBenefitsEnhanced impact Enhanced stiffness
Physical Properties Metric English Comments
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 77
77
ASTM D785
Tensile Strength, Yield 26.2 MPa
3800 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790B
Izod Impact, Notched NB

@Diameter 3.17 mm
NB

@Diameter 0.125 in
bar; ASTM D256
0.534 J/cm

@Diameter 3.00 mm,
Temperature -20.0 °C
1.00 ft-lb/in

@Diameter 0.118 in,
Temperature -4.00 °F
bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C
210 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution