Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos T50-800-01 Polyethylene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos T50-800-01 Polyethylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use properties are required. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.Information provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D4883
Environmental Stress Crack Resistance 5.0 hour
5.0 hour
Condition B, 10%, F50; ASTM D1693
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min; ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Tangent Modulus 1280 MPa
185000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.2 °C
171 °F
ASTM D648
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746
Users viewing this material also viewed the following: