Iran Petrochemical (PCC) EPD 60 R Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) EPD 60 R Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EPD 60 R has a high molecular weight giving it superior toughness even at low temperature. It has excellent heat and detergent resistance.Applications: extrusion blow molding applications include tool boxes, auto motive arts suitcases and large containers.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 0.40 g/10 min
0.40 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Tensile Stress 26.0 MPa
3770 psi
ISO R527
Elongation at Yield 16 %
16 %
ISO R527
Flexural Modulus 1.05 GPa
152 ksi
ISO 178
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 151 °C
304 °F
ISO 306/A
Heat Distortion Temperature 86.0 °C
187 °F
ISO 75/B