Johnson Matthey Mattiflux 100 Brazing Flux Paste

Category Metal , Nonferrous Metal , Solder/Braze Alloy
Manufacturer Johnson Matthey
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey Mattiflux 100 Brazing Flux Paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mattiflux 100 flux paste is a general purpose flux with a good life at temperature and overheat resistance, being active to 1520°F. It is suitable for use with brazing alloys which have a liquidus of up to 1430°F Flux residues can be removed with hot water after brazing. Residues: Water solubleInformation provided by Johnson Matthey.
Thermal Properties Metric English Comments
Active Range 550 - 825 °C
1020 - 1520 °F