Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.44 - 1.50 g/cc
1.44 - 1.50 g/cc
ASTM D 792
ASTM Color -2.83 - -1.23
-2.83 - -1.23
Color A, ME 12
-2.48 - -0.880
-2.48 - -0.880
Color B, ME 12
91.26 - 92.86
91.26 - 92.86
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 82

@Time 15.0 sec
78 - 82

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 27.6 MPa
>= 4000 psi
ASTM D 638
Izod Impact, Notched >= 0.450 J/cm
>= 0.843 ft-lb/in
Method A; ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point >= 80.0 °C
>= 176 °F
ASTM D 1525
Heat Distortion Temperature >= 75.0 °C
>= 167 °F
ASTM D648
Flammability, UL94 V-0
V-0
Descriptive Properties Value Comments
Application General Purpose Profiles