Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kazanorgsintez 102-57 Low Density Polyethylene Composite, for Further Radiation Modification

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Wire/Cable Grade
Manufacturer Kazanorgsintez
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez 102-57 Low Density Polyethylene Composite, for Further Radiation Modification.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: Composition is produced on the basis of 10204-003 base grade low density polyethylene or first and primary grades. Application: Used for heat and radiation resistant wires and cables insulation.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Melt Flow 0.40 - 0.70 g/10 min
0.40 - 0.70 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 8.83 MPa
>= 1280 psi
Elongation at Break >= 550 %
>= 550 %
Tear Strength Test >= 115
>= 115
kgf/cm2
Electrical Properties Metric English Comments
Dielectric Constant <= 2.4

@Frequency 1000 Hz
<= 2.4

@Frequency 1000 Hz
Dielectric Strength >= 40.0 kV/mm
>= 1020 kV/in
Dissipation Factor <= 0.0070

@Frequency 1000 Hz
<= 0.0070

@Frequency 1000 Hz
Descriptive Properties Value Comments
Amount of impurities [pcs] 15
Technological Effectiveness Glib surface; No blowholes or bubbles; Visible to the unaided eye