Kazanorgsintez 175-225 Film Grade Composition of High Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Kazanorgsintez
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez 175-225 Film Grade Composition of High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: Based on polyethylene grades 10803-20, 15803-20, 15813-020,17504-006. Application: Designed for packing manufacture for milk and milk products.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Melt Flow 0.60 - 0.90 g/10 min
0.60 - 0.90 g/10 min
±12%
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 9.80 MPa
>= 1420 psi
Elongation at Break >= 500 %
>= 500 %
Coefficient of Friction, Static 0.10 - 0.25
0.10 - 0.25
Tear Strength Test >= 13.3
>= 13.3
MPa
Descriptive Properties Value Comments
Amount of impurities [pcs] 10
25
to 1m2 of film, from .5 to 1.0 mm incl
5
to 1m2 of film, over 1.0 to 2.0 mm incl