Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Kolon
Trade Name ELLAS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
ASTM D2240
Tensile Strength 44.1 MPa
6400 psi
ASTM D412
Tensile Stress 11.1 MPa

@Strain 100 %
1610 psi

@Strain 100 %
ASTM D412
Elongation at Break 450 %
450 %
ASTM D412
Tear Strength 107 kN/m
611 pli
ASTM D624
Processing Properties Metric English Comments
Nozzle Temperature 190 - 200 °C
374 - 392 °F
Injection Molding
Zone 1 155 - 170 °C
311 - 338 °F
Injection Molding
155 - 170 °C
311 - 338 °F
Extrusion Molding
Zone 2 175 - 190 °C
347 - 374 °F
Extrusion Molding
185 - 190 °C
365 - 374 °F
Injection Molding
Zone 3 175 - 190 °C
347 - 374 °F
Extrusion Molding
185 - 195 °C
365 - 383 °F
Injection Molding
Zone 4 185 - 200 °C
365 - 392 °F
Extrusion Molding
Die Temperature 185 - 195 °C
365 - 383 °F
Extrusion Molding
Head Temperature 190 - 205 °C
374 - 401 °F
Extrusion Molding