Material Notes:
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent chemical resistance, Wide usage temperature, Good impact absorbing characteristics. Information provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
DIN 53479; ASTM D792
Water Absorption 0.90 %
0.90 %
DIN 53475; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
DIN 53505; ASTM D785
Tensile Strength, Ultimate 83.0 MPa
12000 psi
DIN 53455; ASTM D638
Elongation at Break 9.0 %
9.0 %
DIN 53455; ASTM D638
Flexural Yield Strength 137 MPa
19900 psi
DIN 53452; ASTM D790
Flexural Modulus 3.40 GPa
493 ksi
DIN 53452; ASTM D790
Izod Impact, Notched 0.790 J/cm
1.48 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 220 °C
428 °F
DIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
DIN 53461; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
DIN 53461; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149/DIN 53481
Arc Resistance 136 sec
136 sec
ASTM D495
Users viewing this material also viewed the following: