Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical LUTENE LB5000 LDPE Extrusion Coating

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer LG Chemical
Trade Name LUTENE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LUTENE LB5000 LDPE Extrusion Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: LUTENE LB5000 is mainly intended for extrusion coating and can be processed at high speed uniform thickness and width. LUTENE LB5000 is also noted for the excellent adhesion to porous and non porous substrates such as paper, nylon, OPP, PET and aluminum and has good heat seal strength and hot-tack strength. LUTENE LB5000 contains on additives.Main Application: Flexible package( tie layer or sealant layer of laminating film), paper and paper board coating (release paper, paper cup, kraft paper)CAS No. 9002-88-4Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.918 g/cc
0.918 g/cc
ASTM D1505
Water Vapor Transmission 20.0 g/m²/day

@Pressure 0.101 MPa
1.29 g/100 in²/day

@Pressure 14.7 psi
ASTM D393
Melt Flow 5.0 g/10 min

@Load 2.61 kg,
Temperature 190 °C
5.0 g/10 min

@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 43
43
ASTM D2240
Tensile Strength at Break 12.0 MPa
1740 psi
200mm/min; ASTM D638
Tensile Strength, Yield 8.83 MPa
1280 psi
200 mm/min; ASTM D638
Elongation at Break 550 %
550 %
200 mm/min; ASTM D638
Flexural Modulus 0.196 GPa
28.4 ksi
200mm/min; ASTM D790
Thermal Properties Metric English Comments
Melting Point 107 °C
225 °F
10°C/min; DSC
Users viewing this material also viewed the following: