Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LNP ULTEM® JD7904 Polyetherimide  (discontinued **)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LNP ULTEM® JD7904 Polyetherimide  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 84.3 MPa
12200 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 128 MPa
18600 psi
ASTM D790
Flexural Modulus 3.73 GPa
541 ksi
ASTM D790
Izod Impact, Notched 0.290 J/cm
0.543 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 200 °C

@Thickness 3.20 mm
392 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
ASTM D257
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved