Mechanical Properties Metric English Comments
Flexural Modulus 2.20 - 3.20 GPa
319 - 464 ksi
ASTM D790
Prodways PLASTCure Cast 200 3D Printing Polymer
Good reactivity and low viscosity. Outstanding burnout properties with nearly zero ash content.Highly suitable for direct investment casting or dental applications.Information provided by Genistar.
Flexural Modulus 2.20 - 3.20 GPa
319 - 464 ksi
ASTM D790-04
Proto3000 Objet Digital Materials™ DM_8310 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
Flexural Modulus 2.20 - 3.20 GPa
319 - 464 ksi
ASTM D790-04
Proto3000 Objet Digital Materials™ DM_8320 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
Flexural Modulus 2.20 - 3.20 GPa
319 - 464 ksi
ASTM D790-04
Proto3000 Objet Digital Materials™ DM_8330 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide..
Flexural Modulus 2.20 - 3.20 GPa
319 - 464 ksi
ASTM D790-04
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Flexural Modulus 2.20 - 3.20 GPa
319 - 464 ksi
ASTM D790-04
Proto3000 Objet VeroClear FullCure810
Information provided by Proto3000 for their protoyping engineering services.
Flexural Modulus 2.20 - 3.20 GPa
319 - 464 ksi
ASTM D790-04
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Flexural Modulus 2.41 - 3.20 GPa
350 - 464 ksi
Average value: 2.79 GPa Grade Count:14
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate ..
Flexural Modulus 2.80 - 3.20 GPa
406 - 464 ksi
ASTM D790
Loxim 820 12 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
Flexural Modulus 2.80 - 3.20 GPa
406 - 464 ksi
ASTM D790
Loxim 840 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Flexural Modulus 2.07 - 3.20 GPa
300 - 464 ksi
Average value: 2.65 GPa Grade Count:27
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
Flexural Modulus 2.20 - 3.20 GPa
319 - 464 ksi
ASTM D790-04
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer
Information provided by Proto3000 for their protoyping engineering services.
Flexural Modulus 0.620 - 3.20 GPa
89.9 - 464 ksi
Average value: 1.41 GPa Grade Count:154
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..