Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucobit Lucofin® 1412-t3 Polyolefin TPO Granules, Light Grey

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Lucobit AG
Trade Name Lucofin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucobit Lucofin® 1412-t3 Polyolefin TPO Granules, Light Grey.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t3 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and flexibility and resistance to weathering even at low temperatures.Applications:• Colored roof sheeting• Sealing sheeting• Construction profilesThis product is provided with special halogen free fire retardants in order to pass test method 3 of European standard EN 1187.Information provided by Lucobit AG
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ISO 868
Thermal Properties Metric English Comments
Minimum Service Temperature, Air <= -40.0 °C
<= -40.0 °F
Low Temperature Flexural Test; EN 495-5
Processing Properties Metric English Comments
Processing Temperature 150 - 200 °C
302 - 392 °F
Profiles
160 - 230 °C
320 - 446 °F
Membranes
160 - 270 °C
320 - 518 °F
Coatings
Melt Temperature 160 - 220 °C
320 - 428 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F