Material Notes:
Key Features: conventional melt flow, very high modulus, mineral-filled polypropylene copolymer, high rigidity, good impact resistance, good dimensional stability, low foggingApplications: glove box close-outsDescription: Astryn EPKT25M conventional melt flow, mineral-filled polypropylene copolymer has a good balance of stiffness, impact resistance and dimensional stability. It was designed for a variety of non-cosmetic automotive interior applications.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ISO 2577
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ISO 2039-2
Hardness, Shore D 67
67
ISO 868
Tensile Strength, Yield 26.0 MPa
3770 psi
ISO R527
Elongation at Yield 4.0 %
4.0 %
ISO R527
Flexural Modulus 3.30 GPa
479 ksi
ISO 178
Izod Impact, Notched 3.20 J/cm

@Temperature 23.0 °C
5.99 ft-lb/in

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 131 °C
268 °F