Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® NA951080 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA951080 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE NA 951-080 is designed for use as a base resin for compounding material including gas-injected or chemically expanded insulation. NA 951-080 is a natural, low density, medium molecular weight polyethylene resin containing no additives.Processing TechniquesNA 951-080 has been designed to provide excellent processability over a wide range of extrusion conditions, including the low melt temperature requirements of specialty applications like crosslinkable or foam extrusion. Specific recommendations for processing NA 951-080 can be made only when the applications, end use requirements and type of processing equipment are known.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 2.2 g/10 min
2.2 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 11.7 MPa
1700 psi
ASTM D638
Tensile Strength, Yield 10.3 MPa
1500 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<sub>50</sub>; ASTM D746
Electrical Properties Metric English Comments
Dielectric Constant 2.27

@Frequency 1e+6 Hz
2.27

@Frequency 1e+6 Hz
ASTM D1531
Dissipation Factor 0.000060

@Frequency 2.00e+9 Hz
0.000060

@Frequency 2.00e+9 Hz
ASTM D1531
0.000080

@Frequency 1e+6 Hz
0.000080

@Frequency 1e+6 Hz
ASTM D1531
Processing Properties Metric English Comments
Feed Temperature 138 - 149 °C
280 - 300 °F
Zone 2 149 - 163 °C
300 - 325 °F
Zone 3 191 - 204 °C
375 - 400 °F
Zone 4-x 204 - 218 °C
400 - 425 °F
Adapter Temperature 204 - 218 °C
400 - 425 °F
Die Temperature 204 - 218 °C
400 - 425 °F
Melt Temperature 204 - 218 °C
400 - 425 °F