M Cubed Technologies AAC-501 Aluminum alloy-50% Al2O3 Metal Matrix Composite

Category Ceramic , Oxide , Aluminum Oxide , Metal , Metal Matrix Composite
Manufacturer M Cubed Technologies, Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M Cubed Technologies AAC-501 Aluminum alloy-50% Al2O3 Metal Matrix Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Produced using SiC preforms and a patented pressureless infiltration process. High SiC content - very high stiffness and strength. Can be used to make very large, complex shapes. Tight as-formed tolerances; can also be machined. Very low thermal expansion. Good wear resistance and hardness.Information provided by M Cubed Technologies, Inc.
Physical Properties Metric English Comments
Density 3.30 g/cc
0.119 lb/in³
ASTM C135
Mechanical Properties Metric English Comments
Flexural Strength 160 MPa
23200 psi
ASTM C1161
Descriptive Properties Value Comments
Matrix Al Alloy
Particle Reinforcement Al2O3
Vol. % Reinforcement 50