Density 3.30 g/cc
0.119 lb/in³
NanoScale NanoActive® Calcium Oxide
NanoActive CaO is produced using proprietary processes to obtain high specific surface area (over 20 m²/g vs. 1-2 m²/g for standard CaO) with strong affinity towards carbon dioxide and hydrogen su..
Density 3.29 g/cc
0.119 lb/in³
Ferro IP 750 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to..
Density 3.30 g/cc

@Treatment Temp. 1600 °C,
Time 7200 sec
0.119 lb/in³

@Treatment Temp. 2910 °F,
Time 2.00 hour
Fired Density
Magyar Aluminum ALO-DN-2S Alumina
Reactive Alumina
Density 3.30 g/cc

@Treatment Temp. 1600 °C,
Time 7200 sec
0.119 lb/in³

@Treatment Temp. 2910 °F,
Time 2.00 hour
Fired Density
Magyar Aluminum ALO-EL-2S Alumina
Reactive Alumina
Density 3.30 g/cc
0.119 lb/in³
Apparent
Gouda Vuurvast AC 90-5 D Dense Refractory Brick
Description: A special quality with an extra ordinary resistance to alkali and metallurgical slags, a good resistance to thermal cycling, a good volume stability and high strength at high process te..
Density 3.30 g/cc
0.119 lb/in³
Apparent
Gouda Vuurvast ACZ 85-5 D Dense Refractory Brick
Description: Special low porosity quality with excellent resistance against alkali- and metal slags, a good volume stability and a high strength and elasticity at very high temperatures. Application..
Density 3.30 g/cc
0.119 lb/in³
Apparent
Gouda Vuurvast AK 99 S Dense Refractory Brick
Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qu..
Density 3.30 g/cc
0.119 lb/in³
Mo-Sci Corporation GB-40-N Green B Filter Glass
Applications: Lead-free NVIS Green B filter glass for white LED sources.Information provided by Mo-Sci Corporation.
Density 3.30 g/cc
0.119 lb/in³
LATI Latimass 82-02 D030 PA12
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Density 3.30 g/cc
0.119 lb/in³
Schott N-SK5 Glass
Information Provided by SCHOTT North America, Inc.
Density 3.30 g/cc

@Temperature 20.0 °C
0.119 lb/in³

@Temperature 68.0 °F
Solvay Chemicals (CsAlF4) Cesium Tetrafluoroaluminate
Flux for brazing aluminum. Particularly suitable for flame brazing of magnesium-containing aluminum alloys.HS No.: 38109090 /CAS-No.: 39211-00-2Uses: Automotive Sector, Commercial & Residential Ai..
Density 3.30 g/cc
0.119 lb/in³
ASTM C135
M Cubed Technologies AAC-501 Aluminum alloy-50% Al2O3 Metal Matrix Composite
Produced using SiC preforms and a patented pressureless infiltration process. High SiC content - very high stiffness and strength. Can be used to make very large, complex shapes. Tight as-formed to..
Density 3.30 g/cc
0.119 lb/in³
Ceradyne Ceralloy® 1370CS Aluminum Nitride
Features:high thermal conductivityApplications:semiconductor componentsInformation provided by Ceradyne Company
Density 3.30 g/cc
0.119 lb/in³
Ceradyne Ceralloy® 1370DP Aluminum Nitride
Features:high thermal conductivityApplications:semiconductor componentsmicrowave componentsInformation provided by Ceradyne Company
Density 3.30 g/cc
0.119 lb/in³
Ceradyne Ceralloy® 147-31E Sintered Reaction Bonded Silicon Nitride (Si3N4)
Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met..
Density 3.30 g/cc
0.119 lb/in³
Ceradyne Ceralloy® 147-5 Silicon Nitride
Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradyne's..