Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.30 g/cc | 0.119 lb/in³ | |
NanoScale NanoActive® Calcium Oxide NanoActive CaO is produced using proprietary processes to obtain high specific surface area (over 20 m²/g vs. 1-2 m²/g for standard CaO) with strong affinity towards carbon dioxide and hydrogen su.. |
|||
Density | 3.30 g/cc @Treatment Temp. 1600 °C, Time 7200 sec |
0.119 lb/in³ @Treatment Temp. 2910 °F, Time 2.00 hour |
Fired Density |
Magyar Aluminum ALO-DN-2S Alumina Reactive Alumina |
|||
Density | 3.30 g/cc @Treatment Temp. 1600 °C, Time 7200 sec |
0.119 lb/in³ @Treatment Temp. 2910 °F, Time 2.00 hour |
Fired Density |
Magyar Aluminum ALO-EL-2S Alumina Reactive Alumina |
|||
Density | 3.30 g/cc | 0.119 lb/in³ | Apparent |
Gouda Vuurvast AC 90-5 D Dense Refractory Brick Description: A special quality with an extra ordinary resistance to alkali and metallurgical slags, a good resistance to thermal cycling, a good volume stability and high strength at high process te.. |
|||
Density | 3.30 g/cc | 0.119 lb/in³ | Apparent |
Gouda Vuurvast ACZ 85-5 D Dense Refractory Brick Description: Special low porosity quality with excellent resistance against alkali- and metal slags, a good volume stability and a high strength and elasticity at very high temperatures. Application.. |
|||
Density | 3.30 g/cc | 0.119 lb/in³ | Apparent |
Gouda Vuurvast AK 99 S Dense Refractory Brick Description: This high purity alumina quality has a very low porosity and is fired at a temperature of more than 1700°C. The low percentages of SiO2 and Fe2O3 and the improved density make the qu.. |
|||
Density | 3.30 g/cc | 0.119 lb/in³ | |
Mo-Sci Corporation GB-40-N Green B Filter Glass Applications: Lead-free NVIS Green B filter glass for white LED sources.Information provided by Mo-Sci Corporation. |
|||
Density | 3.30 g/cc | 0.119 lb/in³ | |
LATI Latimass 82-02 D030 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Density | 3.30 g/cc | 0.119 lb/in³ | |
Schott N-SK5 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.30 g/cc @Temperature 20.0 °C |
0.119 lb/in³ @Temperature 68.0 °F |
|
Solvay Chemicals (CsAlF4) Cesium Tetrafluoroaluminate Flux for brazing aluminum. Particularly suitable for flame brazing of magnesium-containing aluminum alloys.HS No.: 38109090 /CAS-No.: 39211-00-2Uses: Automotive Sector, Commercial & Residential Ai.. |
|||
Density | 3.30 g/cc | 0.119 lb/in³ | ASTM C135 |
M Cubed Technologies AAC-501 Aluminum alloy-50% Al2O3 Metal Matrix Composite Produced using SiC preforms and a patented pressureless infiltration process. High SiC content - very high stiffness and strength. Can be used to make very large, complex shapes. Tight as-formed to.. |
|||
Density | 3.30 g/cc | 0.119 lb/in³ | |
Ceradyne Ceralloy® 1370CS Aluminum Nitride Features:high thermal conductivityApplications:semiconductor componentsInformation provided by Ceradyne Company |
|||
Density | 3.30 g/cc | 0.119 lb/in³ | |
Ceradyne Ceralloy® 1370DP Aluminum Nitride Features:high thermal conductivityApplications:semiconductor componentsmicrowave componentsInformation provided by Ceradyne Company |
|||
Density | 3.30 g/cc | 0.119 lb/in³ | |
Ceradyne Ceralloy® 147-31E Sintered Reaction Bonded Silicon Nitride (Si3N4) Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met.. |
|||
Density | 3.30 g/cc | 0.119 lb/in³ | |
Ceradyne Ceralloy® 147-5 Silicon Nitride Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradyne's.. |