Material Notes:
• Alternative to high heat ABS resins• For injection molding• Excellent heat and impact resistanceInformation provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D 792
Water Absorption 0.15 %
0.15 %
ASTM D 570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D 955
Melt Flow 4.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D 785
Tensile Strength, Yield 58.0 MPa
8410 psi
ASTM D 638
Elongation at Break 14 %
14 %
ASTM D 638
Flexural Strength 90.0 MPa
13100 psi
ASTM D 790
Flexural Modulus 2.47 GPa
358 ksi
ASTM D 790
Izod Impact, Notched 2.30 J/cm

@Temperature 23.0 °C
4.31 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 123 °C
253 °F
ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
ASTM D 648