Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.30 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
4.31 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded, Method A, 1200 mm Notch Depth; ASTM D648 |
PolyOne Stat-Tech™ ST5220-0004 CP4D EG Black Polypropylene Impact Copolymer (PP Impact Copolymer) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 2.30 J/cm @Temperature -30.0 °C |
4.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific) Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex.. |
|||
Izod Impact, Notched | 2.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
4.31 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ HTX Ultra LA426G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Higher gloss version of Geon HTX Ultra LA426Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426G Black 2880.Information provided by Pol.. |
|||
Izod Impact, Notched | 2.30 J/cm @Temperature -30.0 °C |
4.31 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML7681 PC Copolymer (Asia Pacific) Polycarbonate with high flow, good processability, good impact and thermal properties, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited translucent colors onl.. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256-93a |
Multibase Multi-Pro® 5012 C Black 50% Filler Content Polypropylene Data provided by Multibase. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256-93a |
Multibase Multi-Pro® 5012 C Natural 50% Filler Content Polypropylene This product is well suited to fabricate non-glossy appliance parts, such as a vacuum cleaner canister. It replaces ABS at favorable cost performance characteristics.Data provided by Multibase. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | |
Shell Carilon® DA6L1A10 Polyketone, Lubricated Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DA6L1A10 is a lubricated injection molding grade with mechanical properties which classify it as an.. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256 |
Ineos Nova 850 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Custom colorsApplications: Injection molding or extrusion, Suitable replacement for some engineering resins, Toys, Packaging, Business eq.. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD4271 PC Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD4271 PC (Asia Pacific) Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon PAI grades cannot be molded successfully in molds with undercuts. Torlon 4601 has been formulated to be moldable.. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256A |
LyondellBasell Pro-fax SG702 Polypropylene Impact Copolymer Key Features: excellent cold impact resistance, good stiffness and impact balance, UV stabilizer, polypropylene copolymer resin, injection moldingApplications: automotive interior trim, pet carriers.. |
|||
Izod Impact, Notched | 2.30 J/cm @Temperature 23.0 °C |
4.31 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
MRC Polymers NAXALOY™ 774 ABS + PC Alloy • Alternative to high heat ABS resins• For injection molding• Excellent heat and impact resistanceInformation provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI) Torlon® 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon® PAI grades cannot be molded successfully in molds with undercuts. Torlon® 4601 has been formulated to.. |
|||
Izod Impact, Notched | 2.30 J/cm @Thickness 3.17 mm |
4.31 ft-lb/in @Thickness 0.125 in |
ASTM Test |
Styrolution Terluran® HH-106 ABS Terluran HH-106 is an injection molding ABS grade with high resistance to heat deformation and impact.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Izod Impact, Notched | 2.30 J/cm @Temperature 23.0 °C |
4.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron INSPIREâ„¢ DLGF 9631.01 Z Polypropylene homopolymer, 60% LGF Overview: DLGF 9631.01 Z is based on polypropylene homopolymer and reinforced with 60% by weight of long glass fiber. (PP-LGF 60, Long Glassfiber Granulate). DLGF 9631.01 Z is produced by pultrusion.. |
|||
Izod Impact, Notched | 2.30 J/cm @Temperature 23.0 °C |
4.31 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron MAGNUMâ„¢ 8391 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 8391 ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Izod Impact, Notched | 2.30 J/cm @Temperature 23.0 °C |
4.31 ft-lb/in @Temperature 73.4 °F |
Injection Molded; ASTM D256 |
Styron Magnumâ„¢ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ MED ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass (continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HH180 PPE+PS Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Asia Pacific) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Europe-Africa-Middle East) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Asia Pacific) LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N.. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY ZX06315 PPE+SEBS+Polyolefin (Europe-Africa-Middle East) LNP* Lubriloy* ZX06315 is a compound based on PPE+PS Blend resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Non-Brominated & N.. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TA210SG30 Impact Modified, 30% Glass Fiber Reinforced PA66, DAM 30% Glass Fiber reinforced, Impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD4271 PC (Europe-Africa-Middle East) Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |