Material Notes:
Viscosity Optimized Type
Physical Properties Metric English Comments
Bulk Density <= 0.900 g/cc
<= 0.0325 lb/in³
Brightness >= 90 %
>= 90 %
Whiteness
Oil Absorption <= 16 %
<= 16 %
ml/100g
Particle Size 18 µm
18 µm
d50
45 µm
45 µm
60% max, wet sieve
200 µm
200 µm
0.1% max, wet sieve
Component Elements Properties Metric English Comments
Fe2O3 <= 0.030 %
<= 0.030 %
Na2O <= 0.30 %
<= 0.30 %
SiO2 <= 0.030 %
<= 0.030 %
Processing Properties Metric English Comments
Moisture Content <= 0.30 %
<= 0.30 %
Descriptive Properties Value Comments
Aluminum Hydroxide (%) >99.5
Determined by difference