Material Notes:
BLUE PE82172 is a blue LDPE-based masterbatch containing 30% Phthalocyanine Pigment. It is designed for outdoor products with excellent dyeing strength and weathering resistance. Color Index No.:Blue 15:3Method of Usage: BLUE PE82172 is designed for ease of dispersion and is therefore suitable for direct addition and mixing with plastic resins in mixer, without the necessity of prior drying.Range of Application: BLUE PE82172 is designed for use in LDPE, HDPE, LLDPE and PP for production of films, sheets, plates, hollowing blow molding and direct injection molding in shaper.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
High Load Melt Index 12.1 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12.1 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Descriptive Properties Value Comments
Carrier LDPE
Compatibility LDPE, HDPE, PP and Ethylene copolymer
Pigment Content 30
Users viewing this material also viewed the following: