MetalTek MTEK 65 UNS C90700 Gear Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK 65 UNS C90700 Gear Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Copper-tin alloy with high tensile, yield and compressive strength as well as wear resistance.Applications: Worm gears, steel mill nutsInformation provided by MetalTekCast UNS C90700; Cast Grade C90700; Cast ASTM B427, B505; SAE 65 (Discontinued); Mil QQ-C-390B
Mechanical Properties Metric English Comments
Hardness, Brinell 102
102
500 kg
Tensile Strength, Ultimate >= 240 MPa
>= 34800 psi
Tensile Strength, Yield >= 125 MPa
>= 18100 psi
Elongation at Break >= 10 %
>= 10 %
Component Elements Properties Metric English Comments
Copper, Cu 88.8 %
88.8 %
Phosphorous, P 0.20 %
0.20 %
Tin, Sn 11 %
11 %