Mikro-Technik Reproflon PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Mikro-Technik
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mikro-Technik Reproflon PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reproflon is reclaimed PTFE scraps. The powder can be reused for the usual manufacturing procedures.Information provided by Mikro-Technik GmbH
Physical Properties Metric English Comments
Density 2.16 - 2.20 g/cc
0.0780 - 0.0795 lb/in³
ASTM D792-50
Crystallinity 60 - 85 %
60 - 85 %
X-ray
Mechanical Properties Metric English Comments
Hardness, Shore D 55 - 59
55 - 59
DIN 53 505
Ball Indentation Hardness 30.5 MPa
4420 psi
DIN 53 456
Tensile Strength, Yield 10.3 - 22.5 MPa
1490 - 3260 psi
ISO/R 527E
Elongation at Break 75 - 150 %
75 - 150 %
ISO/R 527
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air -200 °C
-328 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
DIN 53 482
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
DIN 53 482
Dielectric Constant 2.1

@Frequency 50 Hz
2.1

@Frequency 50 Hz
DIN 53 483
2.1

@Frequency 1000 Hz
2.1

@Frequency 1000 Hz
DIN 53 483
2.1

@Frequency 1e+6 Hz
2.1

@Frequency 1e+6 Hz
DIN 53 483
Dielectric Strength 20.0 - 40.0 kV/mm
508 - 1020 kV/in
ASTM D149/15
Dissipation Factor 0.0010

@Frequency 50 Hz
0.0010

@Frequency 50 Hz
tan delta; DIN 53 483
0.0010

@Frequency 1e+6 Hz
0.0010

@Frequency 1e+6 Hz
tan delta; DIN 53 483
0.0010

@Frequency 1000 Hz
0.0010

@Frequency 1000 Hz
DIN 53 483
Users viewing this material also viewed the following: