Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 °C |
5.00 µin/in-°F @Temperature 68.0 °F |
|
Potters Industries Spheriglass® 2024 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 °C |
5.00 µin/in-°F @Temperature 68.0 °F |
|
Potters Industries Spheriglass® 2429 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9300 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9338 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9348 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9350 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9410 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9450 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 30.0 - 300 °C |
5.00 µin/in-°F @Temperature 86.0 - 572 °F |
|
Novum Glass Solid Soda-lime Technical Series Glass Microspheres Solid soda-lime glass microspheres in colorless powder form. Technical Series Microspheres are solid glass microspheres that have a narrow particle size distribution. Used for chromatography, colum.. |
|||
CTE, linear | 9.00 - 140 µm/m-°C @Temperature >=143 °C |
5.00 - 77.8 µin/in-°F @Temperature >=289 °F |
Average value: 94.8 µm/m-°C Grade Count:2 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
CTE, linear | 9.00 - 12.0 µm/m-°C @Temperature -40.0 - 125 °C |
5.00 - 6.67 µin/in-°F @Temperature -40.0 - 257 °F |
IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-8513 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1301-8400 PPS, linear, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 30.0 - 300 °C |
5.00 µin/in-°F @Temperature 86.0 - 572 °F |
|
Mo-Sci Corporation GL-0262 Ni Coated Soda-Lime Glass Spheres Appearance: Solid soda-lime glass microspheres with metallic nickel coatingTypical applications of GL-0262 glass microspheres include: conductive filler for plastic, pigment, and etc.Information pro.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 30.0 - 300 °C |
5.00 µin/in-°F @Temperature 86.0 - 572 °F |
|
Mo-Sci Corporation GL-0275-S Class VI Soda-Lime Spheres Appearance: Solid soda-lime glass microspheres with light green color in powder form.Typical applications of GL0275-S beads including: high temperature spacer material for gauge control, coating, fi.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-0699-1 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 100 °C |
5.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); STA Cold Formable Medium-Strength AlloyFeatures: This binary, age hardening alloy combines the easy formability and weldability of commercially pure titanium with improved mechanical properties, particu.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 100 °C |
5.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 10% Equiaxed Alpha + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 10% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 100 °C |
5.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Elongated Alpha + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Elongated Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 100 °C |
5.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STOA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STOA (885°C/1hr/AC + 705°C/1hr/AC) condition. Other data below are typical of TIMETAL.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 100 °C |
5.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), Typical This entry has typical property data. Other database entries for TIMETAL® 6-2-4-6 have tensile and fatigue data for specific sample conditions.High-Strength, Intermediate Temperature AlloyFeatures.. |
|||
CTE, linear | 9.00 - 36.0 µm/m-°C @Temperature 20.0 - 1000 °C |
5.00 - 20.0 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Goodfellow Potassium Aluminosilicate (Muscovite Mica) Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 1250 °C |
5.00 µin/in-°F @Temperature 68.0 - 2280 °F |
|
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 1000 °C |
5.00 µin/in-°F @Temperature 68.0 - 1830 °F |
|
CeramTec 192/193 Titania 192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 400 °C |
5.00 µin/in-°F @Temperature 68.0 - 752 °F |
|
Zircar Refractory Composites RS-1200 Refractory Sheet ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-12.. |
|||
CTE, linear | 9.00 - 11.0 µm/m-°C @Temperature 1000 °C |
5.00 - 6.11 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CSN-A116 Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | y direction |
Arlon TC600 Glass, PTFE and Micro-Dispersed Ceramic High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-9 Strontium Ferrite Ceramic Magnetic Material |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | y direction |
Arlon AD410 Glass, PTFE and Micro-Dispersed Ceramic High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 °C |
5.00 µin/in-°F @Temperature 68.0 °F |
Longitudinal; ASTM E228 |
Polystrand ThermoPro™ IE7010 Unitape Unidirectional Polypropylene-Glass Composite Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer .. |