Mechanical Properties Metric English Comments
Tensile Strength 1.03 MPa
149 psi
Typical; ASTM D3574-75 Test E
Rogers Corporation Poron® 4701-41-30 Urethane Foam, Soft, Enhanced Sealability
Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements.  Standard available thickness range from 0.031"..
Tensile Strength >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics CHO-SEAL® 6503 Conductive Elastomer
Description: Highest performance in harsh environments; excellent shielding; best choice for corrosion requirements against aluminum.Molded and ExtrudedRoHS CompliantInformation provided by Chomeric..
Tensile Strength >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics CHO-SEAL® 6510 Conductive Elastomer
Extruded onlyInformation provided by Chomerics
Tensile Strength >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics Tecknit NC-Consil® 750 Nickel Coated Graphite Filled Silicone Elastomer
Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil..
Tensile Strength >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics Tecknit NC-Consil® 751 Nickel Coated Graphite Filled Silicone Elastomer
Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil..
Tensile Strength >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics Tecknit NC-Consil® 770 Nickel Coated Graphite Filled Silicone Elastomer
Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil..
Tensile Strength >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics Tecknit NC-Consil® FR750 Nickel Coated Graphite Filled Silicone Elastomer
Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil..
Tensile Strength >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics Tecknit NC-Consil® FR751 Nickel Coated Graphite Filled Silicone Elastomer
Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil..
Tensile Strength >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics ParPHorm® 1800 Non-Conductive Form-in-Place Gasket
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..
Tensile Strength 1.03 MPa
150 psi
Die A; ASTM D412
Monmouth Rubber & Plastics Durafoamâ„¢ C45 Closed Cell Epichlorohydrin
Information provided by Monmouth Rubber & Plastics Corp.
Tensile Strength >= 1.03 MPa
>= 150 psi
Monmouth Rubber & Plastics Durafoamâ„¢ DK5151 NEO/EPDM Polymeric Blend
Information provided by Monmouth Rubber & Plastics Corp.
Tensile Strength >= 1.03 MPa
>= 150 psi
Monmouth Rubber & Plastics Durafoamâ„¢ P391SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..
Tensile Strength >= 1.03 MPa
>= 150 psi
Monmouth Rubber & Plastics Durafoamâ„¢ P392SHD EPDM
Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ..
Tensile Strength >= 1.03 MPa
>= 150 psi
ASTM D412
Parker Chomerics CHO-SEAL® 6502 Conductive Elastomer
Description: Highest performance in harsh environments; excellent shielding; best choice for corrosion requirements against aluminum.Molded and ExtrudedRoHS CompliantInformation provided by Chomeric..