Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable 3201-xx05D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Network Polymers Softflex® 6080 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3725 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746-79 |
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Uncured Carbon Black Filled Compound
& Carbon black compound with 100 parts Hypalon; 100 parts carbon black; 4 parts magnesia; and 1.5 parts propylene glycol. Physical property data below (except mooney viscosity) are for uncured film. .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WR7400L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Lushan PF-3 Adhesive Resin for Coextruded Multi-layer Barrier Packaging Film Adhesive resin Lushan series for multi-layer barrier food packaging film has durable bonding properties when adheres to Polarity materials, such as PE, PP and PA, EVOH, etc. Adhesive resin Lushan se.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Multibase Multi-Flex® A 9702 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex APEX® 1519-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMForms-PelletsFeatures- Good flexibility Information provided by Teknor Apex Company |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex APEX® 3201-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex APEX® 3301-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 3500-55 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 3501-55-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 9100-65 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 9602-72 Polyvinyl Chloride, Elastomer Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility; Sunlight Resistant (720 hours) Uses Cable Jacketing Wire Types: SEOW; SEW; SJEOW;.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Brittleness Temperature | <= -50.0 °C | <= -58.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-1654A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | JIS K6301 |
Toyobo PELPRENE™ S9001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D 746 |
Zylog Neoplast® 240 FT EB Thermoplastic Vulcanizate Neoplast 240 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D-746 |
Axiall 59996J Moldings & Extrusions Flexible PVC Injection and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | <= -50.0 °C | <= -58.0 °F | ASTM D726 |
Arkema Group LOTADER® 3200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 3200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties, LOTADER 3200 is used in pipeline .. |
|||
Brittleness Temperature | <= -50.0 °C | <= -58.0 °F | ASTM D726 |
Arkema Group LOTADER® 4210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 4210 is a versatile adhesive for extrusion coating or lam.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 1008-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1008-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | |
A. Schulman POLYTROPE™ TPP 504 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 |
DuPont Performance Polymers Kalrez® 4079 FFKM Perfluoroelastomer A low compression set compound for general-purpose use in O-rings, diaphragms, seals, and other parts used in the process and aircraft industries. It is a carbon black-filled compound with excellen.. |