Material Notes:
Multi-Flex® A 8103 is an acoustic barrier compound that meets general motors specification GM2212M(FBMS 4-10). This specification is for a low flexural modulus product. The burn rate is 0.9 in/min (22.5 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.83 g/cc
0.0661 lb/in³
ASTM D792
Melt Flow 5.0 g/10 min
5.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
10 sec; ASTM D-2240
Tensile Strength, Ultimate 2.90 MPa
421 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Strength 64.8 MPa
9400 psi
Flexural Modulus 0.0628 GPa
9.11 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 26.3 kN/m
150 pli
ASTM D624