Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mytex Polymers AN16L(W)-D56 Polypropylene, Talc filled, Compounded, Elastomer, Impact modified

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Talc Filler
Manufacturer Mytex Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mytex Polymers AN16L(W)-D56 Polypropylene, Talc filled, Compounded, Elastomer, Impact modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: AN16L-D56 is a compounded talc filled elastomer modified polypropylene with good impact and excellent material flow properties.Key Applications: Automotive exteriorInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Melt Flow 17 g/10 min
17 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 105 MPa
15200 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 19.0 MPa
2760 psi
50 mm/min; ASTM D638
Flexural Strength 23.0 MPa
3340 psi
Max load; 1.3 mm/min; ASTM D790
Flexural Modulus 1.15 GPa
167 ksi
Tangent; 1.3 mm/min; ASTM D790
Izod Impact, Notched 4.50 J/cm

@Temperature 23.0 °C
8.43 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648